Temperature Dependence of the Tensile Properties of Single Walled Carbon Nanotubes: O(N) Tight Binding MD Simulation

G. Dereli and B. Sungu (Yildiz Tech. Univ.
Istanbul)

Tekin Dereli update to 2009-11-13

https://arxiv.org/abs/0704.0183
This paper examines the effect of temperature on the structural stability andmechanical properties of 20 layered (10,10) single walled carbon nanotubes(SWCNTs) under tensile loading using an O(N) tight binding molecular dynamics(TBMD) simulation method. We observed that (10,10) tube can sustain itsstructural stability for the strain values of 0.23 in elongation and 0.06 incompression at 300K. Bond breaking strain value decreases with increasingtemperature under streching but not under compression. The elastic limit,Young's modulus, tensile strength and Poisson ratio are calculated as 0.10,0.395 TPa, 83.23 GPa, 0.285, respectively, at 300K. In the temperature rangefrom 300K to 900K; Young's modulus and the tensile strengths are decreasingwith increasing temperature while the Poisson ratio is increasing. At highertemperatures, Young's modulus starts to increase while the Poisson ratio andtensile strength decrease. In the temperature range from 1200K to 1800K, theSWCNT is already deformed and softened. Applying strain on these deformed andsoftened SWCNTs do not follow the same pattern as in the temperature range of300K to 900K.

journal: None

category: cond-mat.mtrl-sci

单壁碳拉伸性能的温度依赖性 纳米管:O(N) 紧密结合 MD 模拟

G. Dereli and B. Sungu (Yildiz Tech. Univ.
Istanbul)

Tekin Dereli update to 2009-11-13

https://arxiv.org/abs/0704.0183
本文使用 O(N) 紧密结合分子动力学 (TBMD) 模拟方法研究了温度对 20 层 (10,10) 单壁碳纳米管 (SWCNT) 在拉伸载荷下的结构稳定性和机械性能的影响。我们观察到 (10,10) 管在 300K 时可以维持其结构稳定性,拉伸应变值为 0.23,压缩应变值为 0.06。断键应变值在拉伸下随温度升高而降低,但在压缩下则不然。弹性极限、杨氏模量、拉伸强度和泊松比在 300K 下计算分别为 0.10、0.395 TPa、83.23 GPa、0.285。在300K到900K的温度范围内;杨氏模量和拉伸强度随着温度的升高而降低,而泊松比在增加。在较高温度下,杨氏模量开始增加,而泊松比和抗拉强度降低。在1200K到1800K的温度范围内,SWCNT已经变形和软化。对这些变形和软化的 SWCNT 施加应变与在 300K 到 900K 的温度范围内不遵循相同的模式。